Inconel 660 / Alloy 660 (UNS S66286 / SUH660 / GH2132) – Superalloy Iron Inotsigira Mvura Yakawanda Yekushandisa Pakupisa Kwakanyanya

Tsananguro pfupi:

Inconel 660 (UNS S66286 / SUH660 / GH2132 /W.Nr. 1.4980) isimbi inoomesesa inogadziriswa nemvura ine simba guru uye inodzivirira kupisa kusvika ku704°C (1300°F). Womic Steel inopa Inconel 660 mumhando dzakasiyana dzezvigadzirwa zvinosanganisira pombi isina musono, pombi yakasungirirwa, simbi ine simbi, plate yesimbi, coil yesimbi, strip, flanges, fittings, forgings, waya, uye fasteners dzekushandisa mudenga, turbine yegesi, mota, nuclear, uye petrochemical.


Ruzivo rweChigadzirwa

Matagi eChigadzirwa

Chii chinonzi Inconel 660?

Inconel 660 isimbi ine nickel-chromium superalloy inosimbiswa nekunaya kwe γ' [Ni₃(Al,Ti)] phase panguva yekupisa kwekukwegura. Chiumbwa ichi chine 24-27% nickel, 13.5-16% chromium, uye titanium (1.9-2.35%), aluminium (0.10-0.35%), molybdenum (1.0-1.5%), uye vanadium (0.10-0.50%). Yakagadzirirwa kushandiswa kunoda simba rakawanda kusvika 700°C uye inodzivirira kuoxidation uye ngura zvakanaka.

Giredhi 660 rinozivikanwa ne:

●Simba rekupisa kwakanyanyakusvika 704°C (1300°F)

●Kudzivirira kukwira nekukwira kwakanyanyapakupisa kwakakwirira

●Mvura inonaya inoomakuburikidza nekurapwa kwekupisa kwekukwegura kwakajairika

●Kudzivirira kwakanaka kwe oxidationkusvika 815°C

●Kuramba kuzorora mupfungwapakupisa kwakanyanya

●Isina maginetizvivakwa

●Kugadzirwa kwakanakauye kugona kushanda

Kuumbwa kweMakemikari

Chinhu UNS S66286 (ASTM) SUH660 (JIS) GH2132 (GB) Basa
Nickel (Ni) 24.0 – 27.0 24.0 – 27.0 24.0 – 27.0 Chinosimbisa ngura cheAustenite, kuramba ngura
Chromium (Cr) 13.5 – 16.0 13.5 – 16.0 13.5 – 16.0 Kuramba kwe oxidation, carbide yekare
Molybdenum (Mo) 1.0 – 1.5 1.0 – 1.5 1.0 – 1.5 Kusimbisa mhinduro yakasimba
Titanium (Ti) 1.90 – 2.35 1.90 – 2.35 1.90 – 2.35 mvura inonaya ne γ, kuoma kwezera
Aruminiyamu (Al) 0.10 – 0.35 ≤ 0.35 ≤ 0.35 kunaya kwemvura kwe γ'
Vanadium (V) 0.10 – 0.50 0.10 – 0.50 0.10 – 0.50 Kucheneswa kwezviyo, carbide yekare
Boron (B) 0.003 – 0.010 0.001 – 0.010 0.001 – 0.010 Kusimbisa muganhu wezviyo
Cobalt (Ko) ≤ 1.00 ≤ 1.00 ≤ 1.00 Chinhu chasara
Simbi (Fe) Kuenzana Kuenzana Kuenzana Chinhu chepakutanga
Kabhoni (C) ≤ 0.08 ≤ 0.08 ≤ 0.08 Carbide yekare
Silikoni (Si) ≤ 1.00 ≤ 1.00 ≤ 1.00 Deoxidizer
Manganese (Mn) ≤ 2.00 ≤ 2.00 ≤ 2.00 Deoxidizer
Phosphorus (P) ≤ 0.025 ≤ 0.040 ≤ 0.030 Kusachena
Sarufa (S) ≤ 0.025 ≤ 0.030 ≤ 0.020 Kusachena

Zvivakwa zveMichina

Dambudziko reAnnaled (Mhinduro Yakarapwa)

Pfuma ASTM A453 Giredhi 660 Kukosha
Simba reKusimba ≤ 724 MPa (105 ksi)  
Simba reKubereka (0.2% Kuderedzwa) –  
Kureba ≥ 25%  
Kuoma ≤ 91 HRB

Kukwegura (Kuoma kwemvura)

Pfuma ASTM A453 Giredhi 660 Zvakajairika Zvakaitwa
Simba reKusimba ≥ 965 MPa (140 ksi) 1,000 – 1,100 MPa
Simba reKubereka (0.2% Kuderedzwa) ≥ 655 MPa (95 ksi) 700 – 800 MPa
Kureba ≥ 15% 18 - 25%
Kuoma 24 - 35 HRC 28 - 32 HRC
Simba reKukwira (650°C, 100h) ≈ 240 MPa  
Simba reKukwira (700°C, 100h) ≈ 210 MPa

Zvimiro zvemuviri

Pfuma Kukosha
Kuwanda kwevanhu 7.95 g/cm³
Nzvimbo Yekunyunguduka 1371 – 1427°C
Kufambisa kwekupisa 15.0 W/m·K pa150°C
Kuwanda kweThermal Coefficient 16.8 × 10⁻⁶/°C (20-100°C)
Modulus yeElastic 201 GPa
Kubvumidzwa kweMagineti Isina magineti

Mabhenefiti Akakosha eInconel 660

Simba reKupisa Kwakakwirira– Inconel 660 inochengetedza simba rakasimba rekudhonza, kuneta, uye kukwira-svetuka kusvika ku704°C. Nzira yekusimbisa mvura yeγ' inopa simba rakakwirira rekupisa kana tichienzanisa nesimbi dzisina ngura dzinoshandiswa neaustenitic. Chiumbwa ichi chinowanzoshandiswa pamabhaudhi eturbine nezvinosunga uko kudzivirira kudzikama kwakakosha.

Kuramba Kunoputika Kwakanaka– Chiumbwa ichi chinoratidza kusimba kukuru pakukwira kwemvura kana tembiricha yakakwira. Hupenyu hwemvura inokwira nekukwira pa650°C hunopfuura maawa chiuru kana paine kumanikidzwa kuri pakati nepakati, zvichiita kuti ive chinhu chakavimbika chekushandisa kwenguva refu pakupisa kwakanyanya.

Kuoxidation Yakanaka uye Kuramba Kuora– Iine 13.5-16% chromium, Inconel 660 inopa hudziviriro hwakanaka kuokisijeni, kukura, uye ngura inodziya zvakanyanya. Chiumbwa ichi chinoshanda zvakanaka munzvimbo dzinookisijeni kusvika ku815°C uye chinodzivirira ngura dzakasiyana-siyana.

Mvura Inoomarara– Inconel 660 inogona kuomarara nekupiswa nekukwegura. Kureba kwenguva (675-705°C, maawa 12-16) kunovandudza hunhu hwakanaka hwemakanika uye kunopa simba rakanaka rekudzivirira kushushikana, izvo zvakakosha pakushandisa mabhomba.

Kuramba Kuneta Kwakanaka- Chiumbwa ichi chinopa simba rakanakisisa rekudzivirira kuneta uye kuneta kwekupisa, zvichiita kuti chikwanise kushandiswa nezvinhu zvinogona kudzokororwa kana tembiricha yakakwira. Izvi zvakakosha zvikuru pakushandiswa kweturbine uye zvikamu zveinjini.

Kushanda Kwakanaka Uye Kugona Kugadzira Machina– Inconel 660 ine michina iri nani kupfuura mamwe ma superalloys akawanda. Inogona kugadzirwa zviri nyore, kushandiswa kupisa, uye kushandiswa kutonhora. Chiumbwa ichi chinonamirwa uchishandisa TIG, MIG, uye resistance welding nesimbi dzakakodzera.

Mabhenefiti Akakosha eInconel 660

Simba reKupisa Kwakakwirira– Inconel 660 inochengetedza simba rakasimba rekudhonza, kuneta, uye kukwira-svetuka kusvika ku704°C. Nzira yekusimbisa mvura yeγ' inopa simba rakakwirira rekupisa kana tichienzanisa nesimbi dzisina ngura dzinoshandiswa neaustenitic. Chiumbwa ichi chinowanzoshandiswa pamabhaudhi eturbine nezvinosunga uko kudzivirira kudzikama kwakakosha.

Kuramba Kunoputika Kwakanaka– Chiumbwa ichi chinoratidza kusimba kukuru pakukwira kwemvura kana tembiricha yakakwira. Hupenyu hwemvura inokwira nekukwira pa650°C hunopfuura maawa chiuru kana paine kumanikidzwa kuri pakati nepakati, zvichiita kuti ive chinhu chakavimbika chekushandisa kwenguva refu pakupisa kwakanyanya.

Kuoxidation Yakanaka uye Kuramba Kuora– Iine 13.5-16% chromium, Inconel 660 inopa hudziviriro hwakanaka kuokisijeni, kukura, uye ngura inodziya zvakanyanya. Chiumbwa ichi chinoshanda zvakanaka munzvimbo dzinookisijeni kusvika ku815°C uye chinodzivirira ngura dzakasiyana-siyana.

Mvura Inoomarara– Inconel 660 inogona kuomarara nekupiswa nekukwegura. Kureba kwenguva (675-705°C, maawa 12-16) kunovandudza hunhu hwakanaka hwemakanika uye kunopa simba rakanaka rekudzivirira kushushikana, izvo zvakakosha pakushandisa mabhomba.

Kuramba Kuneta Kwakanaka- Chiumbwa ichi chinopa simba rakanakisisa rekudzivirira kuneta uye kuneta kwekupisa, zvichiita kuti chikwanise kushandiswa nezvinhu zvinogona kudzokororwa kana tembiricha yakakwira. Izvi zvakakosha zvikuru pakushandiswa kweturbine uye zvikamu zveinjini.

Kushanda Kwakanaka Uye Kugona Kugadzira Machina– Inconel 660 ine michina iri nani kupfuura mamwe ma superalloys akawanda. Inogona kugadzirwa zviri nyore, kushandiswa kupisa, uye kushandiswa kutonhora. Chiumbwa ichi chinonamirwa uchishandisa TIG, MIG, uye resistance welding nesimbi dzakakodzera.

Kurapa Kupisa kweInconel 660

Inconel 660 isimbi inoomarara inonamira mvura inoda kurapwa kwakanyatsonaka kwekupisa kuti iwane hunhu hwakanaka hwemakanika:

Kunyungudutsa kweMhinduro (Chimiro A):

●Tembiricha:980 – 1010°C (1800 – 1850°F)

●Nguva Yokunyikisa:awa imwe chete

●Kutonhodza:Kutonhora nekukurumidza (kudzima mafuta kana mvura)

●Chinangwa:Nyungudutsa zvese zvinokonzeresa mvura, zadzisa austenite yechikamu chimwe chete

●Mhedzisiro:Mamiriro akapfava, anoshanda, akagadzirira kugadzirwa uye kugadzirwa

Kuoma kwemvura (Kukwegura - Mamiriro B):

●Tembiricha:675 – 705°C (1250 – 1300°F)

●Nguva Yokunyikisa:Maawa gumi nemaviri kusvika gumi nematanhatu

●Kutonhodza:Mhepo inotonhorera

●Chinangwa:Fomu Ni₃(Al,Ti) γ' inonaya yekusimbisa

●Mhedzisiro:Simba guru uye kuramba kukwira

Kukwegura Kaviri (Imwe nzira):

● Danho Rokutanga: 705°C kwemaawa gumi nematanhatu, vira rinotonhorera kusvika 620°C

● Danho rechipiri: 620°C kwemaawa gumi nematanhatu, inotonhorera nemhepo

●Chinangwa:Gadzirisa kuramba kushushikana kwekushandisa bolting applications

Mafomu Ezvigadzirwa Anowanikwa kubva kuWomic Steel

Pombi Isina Musono & Tube Isina Musono

●Dhayamita yekunze:6mm – 200mm

●Ukobvu hwemadziro:1mm – 25mm

●Kureba:Kusvika 12m

●Mitemo:ASTM B639, ASTM B983, AMS 5731, AMS 5732, AMS 5737, AMS 5895

●Mashandisirwo:Mapombi ekupisa kwakanyanya, machubhu ekupisa, mitsetse yemidziyo, machubhu emuchadenga

●Mazwi akakosha:Pombi isina musono yeInconel 660, chubhu yeGiredhi 660, pombi yeUNS S66286, chubhu yeSUH660, pombi isina musono 1.4980

Bhawa reSimbi (Rakatenderera, Sikweya, Rakatsetseka, Hex)

●Dhayamita:6mm – 300mm

●Pamusoro:Yakamonerwa inopisa, Yakajeka (yakadhonzwa ichitonhora), Yakagayiwa pasi, Yakatenderedzwa

●Mitemo:ASTM A453, ASTM B639, AMS 5731, AMS 5732, AMS 5734, AMS 5737

●Mashandisirwo:Mabhaudhi eturbine, zvisungo, mastuds, shafts, ma valvu stems, machine stock

●Mazwi akakosha:Bhawa rakatenderera reInconel 660, Bhawa reGiredhi 660, tsvimbo yeSUH660, ASTM A453 Giredhi 660, zvinosunga tembiricha yepamusoro

Plate yeSimbi & Sheet

●Ukobvu:1mm – 100mm

●Upamhi:Kusvika 2000mm

●Mitemo:AMS 5525, AMS 5858

●Mashandisirwo:Zvikamu zvemidziyo yekumanikidza, zvikamu zvechimiro, nzvimbo dzisina chinhu dzeflange

●Mazwi akakosha:Purati yeInconel 660, pepa reGiredhi 660, plate ye alloy, plate yekupisa kwakanyanya

Simbi Coil & Strip

●Ukobvu:0.5mm – 4.0mm

●Upamhi:10mm – 1000mm

●Mitemo:AMS 5525

●Mashandisirwo:Zvikamu zvakagadzirwa, maburi, zvidhindo

●Mazwi akakosha:Inconel 660 coil, strip, strip yekupisa kwakanyanya

Flanges & Fittings

●Mhando:Welding Mutsipa, Slip-On, Bofu, Socket Welding, Threaded

●Saizi:1/2" – 24"

●Kuyera Kumanikidzwa:Kirasi 150 - Kirasi 2500

●Mitemo:ASTM A453, ASME B16.5

●Mazwi akakosha:Inconel 660 flanges, zvigadziko zveGiredhi 660

Zvekushongedza

●Mhando:Mhete, madhisiki, miseve, miviri yevharuvhu, majometri akagadzirwa

●Kurema:Kusvika 3,000kg pachidimbu chimwe nechimwe

●Mitemo:ASTM A453, AMS 5731

●Mazwi akakosha:Inconel 660 yekuumba, mhete yekuumba, yekuumba zvikamu zveturbine

Zvisungo (Mabhoti, Nzungu, Mapfundo)

●Mhando:Mabhaudhi eHex, Zvikushi zveSocket head cap, Mabhaudhi eStud, Zvitanda zvakarukwa, Nuts, Mawashers

●Saizi:M2 – M100, 1/4" – 4"

●Mitemo:ASTM A453 Giredhi 660, ASTM B637

●Mashandisirwo:Mabhaudhi eturbine, kubatana kweflange inodziya zvakanyanya, zvinosunga zvechimiro

●Mazwi akakosha:Mabhaudhi eInconel 660, Mabhaudhi eGiredhi 660, zvinosunga tembiricha yepamusoro, mabhaudhi eturbine

Mavharuvhu eGiredhi 660

●Mhando:Mavharuvhu ebhora, Mavharuvhu egedhi, Mavharuvhu eglobe, Mavharuvhu ekutarisa

●Saizi:1/2" – 12"

●Kuyera Kumanikidzwa:Kirasi 150 - Kirasi 2500

●Kureba kweTembiricha:-196°C kusvika +704°C

●Maitiro Ekugadzira:API 608, API 6D, ASME B16.34

●Kuita:Manual, Pneumatic, Magetsi

●Mashandisirwo:Kuparadzaniswa kwemaitiro ekupisa kwakanyanya, mitsetse yemhepo yeturbine, kudzora turbine yegesi

Giredhi 660 vs. Inconel 718: Kuenzanisa

Inconel 660 naInconel 718 ese ari maviri ma superalloys anoomesa mvura, asi ane musiyano wakasiyana:

Inconel 660 - Chishongo chesimbi chinobva pakupisa kwakanyanya

●Chikamu Chekutanga:Iron (yakaenzana) ine 24-27% Ni

●Chikamu chekusimbisa:γ' (Ni₃(Al,Ti))

●Simba reKusimba (rakura):≥ 965 MPa

●Kugona kupisa:Kusvika 704°C

●Zvishandiso zvikuru:Mabhaudhi eturbine, zvisungo, mastuds, zvikamu zveinjini yejeti

●Mutengo:Yakachipa kupfuura 718 yakagadzirwa nenickel

●Inconel 718 - Superalloy Yakavakirwa paNickel

●Chikamu Chekutanga:Nickel (50-55%) ine 18-20% Fe

●Matanho ekusimbisa:γ' (Ni₃Al) + γ'' (Ni₃Nb)

●Simba reKusimba (rakura):≥ 1,240 MPa

●Kugona kupisa:Kusvika 700°C

●Zvishandiso zvikuru:Madhisiki eturbine, mota dzeroketi, mafuta negesi zveHPHT

Nguva yekusarudza Giredhi 660:Mashandisirwo anoda mabhaudhi ekupisa kwakanyanya, zvikamu zveinjini yejet, mabhaudhi eturbine, uye mota inoshanda zvakanyanya uko mutengo unoenderana uye simba rakawanda rinosvika 700°C rinodiwa.

Nguva yekusarudza Inconel 718:Mashandisirwo anoda simba guru rekupisa kwepamusoro-soro, kusimba kwekutyoka, uye kuramba kukwira kwemvura pakupisa kunosvika 700°C uko kusingakoshi mari yakawanda.

Mitemo & Magadzirirwo

Zvakajairika Tsananguro
Kusarudzwa kweUNS S66286
Nhamba yeWerkstoff 1.4980
AISI/SAE 660
ASTM A453 Tsananguro yakajairika yebholting inodziya zvakanyanya
ASTM B639 Bhaa/tsvimbo yesimbi inodziya zvakanyanya
AMS 5525 Ndiro/pepa/chidimbu
AMS 5731 Bhawa, waya, maforging
AMS 5732 Bhawa, waya, maforging
AMS 5734 Bhawa, waya, maforging
AMS 5737 Pombi nechubhu
AMS 5895 Bhawa, waya, maforging
JIS SUH660
GB/T GH2132
wekuEurope 1.4980 / X6NiCrTiMoV25-15-2
ISO X6NiCrTiMoV25-15-2

Mashandisirwo eInconel 660

Muchadenga– Inconel 660 inoshandiswa zvakanyanya muzvikamu zvejet engine negas turbine zvinosanganisira turbine bolts, compressor disks, turbine casings, afterburner parts, thrust reversers, uye engine mounting hardware. Musanganiswa wayo wesimba rekupisa kwakanyanya, kuramba kuneta, uye kuramba oxidation kunoita kuti ive yakakodzera kushandiswa kwakakosha mundege. Chiumbwa ichi chinhu chakajairika chejet engine bolts uye fasteners dzinoshanda patembiricha inosvika 700°C.

Kugadzira Simba reTurbine yeGasi– Chiumbwa ichi chinoshandiswa pakugadzira mabhaudhi emagetsi, ma studs, uye zvinosungirirwa muma turbine egasi emaindasitiri, ma turbine emhepo, uye ma power plant akabatana. Kusagadzikana kwayo pakumanikidzwa pakupisa kwakakwirira kunoita kuti mabhaudhi akwanise kusimbiswa kuburikidza nehupenyu hwebasa hwakareba.

Mota– Inconel 660 inoshandiswa muzvigadziko zve turbocharger, manifold exhaust, zvikamu zveinjini yedhiziri, uye zvisungo zvemotokari zvinoshanda zvakanyanya. Kugona kwayo kutsungirira tembiricha yegesi inobuda mumhepo uye kupisa kunoita kuti ikodzere mainjini emazuva ano anoshanda zvakanyanya uye ane turbocharger.

Simba reNyukireya- Chiumbwa ichi chinoshandiswa muzvikamu zvenyukireya, mukati memukati, nzira dzekutonga tsvimbo, uye zvisungo zvekupisa zvakanyanya zvinoda kuvimbika kwenguva refu uye kuramba kupiswa nemwaranzi ye neutron.

Kugadziriswa kwePetrokemikari– Inconel 660 inoshandiswa mumakemikoro emakemikari anodziya zvakanyanya, machubhu ekugadzirisa, zvikamu zvefurnace, uye mapaipi ekugadzira anoda simba uye kuramba kuoxidation pakupisa kwakakwira.

Kurovera Kwepamusoro-soro– Giredhi 660 ndiyo midziyo yakajairika yekushandisa mabhoti ekupisa kwakanyanya. Mabhoti nema stud zveASTM A453 Giredhi 660 zvakatsanangurwa zvakanyanya kune ma flange emidziyo yepressure, ma turbine casings, uye ma connection emapaipi ekupisa kwakanyanya anoda kudzivirira kukambaira uye kuzorora kwekushushikana.

Mibvunzo Inowanzo bvunzwa

Mubvunzo: Chii chinonzi Inconel 660?

A: Inconel 660 (UNS S66286 / SUH660 / GH2132) isimbi inosimbisa simba rekupisa rinosvika 704°C. Inosimbiswa nemvura inonaya neγ' kuburikidza nekupisa kwekare uye inoshandiswa zvakanyanya pamabhaudhi eturbine, zvinosunga, uye zvikamu zveinjini yejeti.

Mubvunzo: Musiyano uripo pakati peGiredhi 660 neInconel 718 ndeupi?

A: Inconel 660 yakagadzirwa nesimbi (ine 24-27% Ni, Fe yakayerwa) ine simba rekudhonza ≥ 965 MPa, nepo Inconel 718 yakagadzirwa nenickel (50-55% Ni) ine simba rekudhonza ≥ 1,240 MPa. Giredhi 660 isingadhuri zvakanyanya uye inoshandiswa zvakanyanya pakubolta; Inconel 718 inoshandiswa pakushandisa simba guru.

Mubvunzo: Ndeipi tembiricha yepamusoro yebasa reInconel 660?

A: Inconel 660 yakayerwa kuti irambe ichishandiswa kusvika 704°C (1300°F). Kana paine kusakwanisa kuoxidation, kufamba kwenguva pfupi kusvika 815°C (1500°F) kunogoneka. Simba rekufamba rinoderera zvakanyanya kupfuura 700°C.

Mubvunzo: Ko Inconel 660 inonamirwa nyore here?

A: Ehe, Inconel 660 inogona kusungirirwa uchishandisa TIG, MIG, uye maitiro ekudzivirira kusungirirwa. Zvisinei, kusungirirwa kunoda kungwarira kudzora kupisa uye kusarudza simbi yekuzadza kuti isapwanyike. Kupwanya kwemvura mushure mekusungirirwa uye kukwegura kunogona kudiwa kuti udzorere hunhu hwemakanika.

Mubvunzo: Ndezvipi zvinorehwa neInconel 660 muchiChinese?

A: Nhamba yekuChina yakaenzana neInconel 660 iGH2132 (高温合金) yekushandiswa kwendege nemhepo uye tembiricha yepamusoro, uye yakaenzana neyavaJapan ndiSUH660.

Mubvunzo: Ndeapi mafomu ezvigadzirwa anowanikwa eInconel 660?

A: Womic Steel inopa Inconel 660 mupombi isina musono, pombi yakasungirirwa, simbi yakaganhurirwa, ndiro yesimbi, coil yesimbi, strip, flanges, fittings, forgings, waya, fasteners, uye mavharuvhu. Tsanangudzo yakazara yechigadzirwa uye saizi dzakanyorwa muchikamu chekuwanikwa kwechigadzirwa.

Mubvunzo: Ko Inconel 660 inoda kurapwa nekupisa here?

A: Ehe. Inconel 660 inoda solution annealing (980-1010°C) ichiteverwa nekukwegura (675-705°C kwemaawa 12-16) kuti iwane hunhu hwakanaka hwemuchina. Kurapa kwekukwegura kunoita kuti γ' irambe yakasimba.

Bata Womic Steel

Webhusaiti: www.womicsteel.com
E-mail: sales@womicsteel.com

Nhare / WhatsApp / WeChat:

Victor: +86 15575100681

Jack: +86 18390957568

Womic Steel – Mubatsiri wako wakavimbika weInconel 660 / Grade 660 (UNS S66286, SUH660, GH2132) pombi isina musono, simbi bar, simbi plate, simbi coil, flanges, fittings, forgings, uye fasteners dzekushandisa aerospace, gas turbine, kugadzira magetsi, uye high-temperature bolting pasi rese. Kutevedza kwakazara, classification society certification, uye EN 10204 Type 3.1/3.2 magwaro aripo.